The application of PVC foam board is relatively common, most of which are used for skid resistance, fall prevention, pressure prevention, heat insulation and heat preservation of blocks. PVC foam board has many colors, among which there are a lot of milky white ones, because milky white looks more beautiful and generous.
Now customers have high regulations on the whiteness of foam board. We all know that no matter what it is, if it is milky white, it is easy to turn yellow, as is the case with PVC foam board. Many manufacturers add fluorescent whitening agent to improve whiteness, so which PVC foaming fluorescent whitening agent is better?
Sometimes people see that the appearance of many articles is very white and bright. In fact, they were not like that at that time. Their initial situation was a little yellow. Only when some organic chemical additives were added in the production process can they look particularly white.
Among them, PVC products are not very white. They are easy to be oxidized by air in the gas, resulting in a dull appearance. Many manufacturers also consider trying to use fluorescent brighteners to improve the whiteness value.
However, the fluorescent brighteners on the market at this stage can be said to be very poor. Either the price is relatively high, or some agents can gain a lot of profits by increasing the price to reduce the water content.
This agent tried his best, but the actual effect of many fluorescent whitening agents coming to the plastic manufacturers has long been conceivable. That also made many plastic manufacturers eliminate the idea of looking for fluorescent brighteners.
However, there is no need to worry about this. Because a fluorescent whitening agent, RQT-C-1, is a special PVC foaming fluorescent whitening agent, can completely solve this series of problems, and there is no need to worry about the water content.
This fluorescent whitening agent can be evenly mixed with the raw materials at the time of manufacturing the foam board. One ton of raw materials only need to add about 200g. According to the high temperature thermal melting, it can better maintain the resin powder from being oxidized and discolored by air. The whiteness value of the exported products can be increased by about 15 points according to the whiteness meter inspection, and the overall appearance color looks more mellow.